@omtilakpol17053 ай бұрын
Using direct cement sand mortor will shrink itself while curing, and will have cracks in future. Instead use polymer modified mortor having minimum compression strength of 40 Nmm^2.
@user-wr1dr9mk8r18 күн бұрын
প্রতিটা কেমিক্যালের নাম আপনি যদি লিখে দিতেন তাহলে খুবই ভালো হতো
@RawatSafe2 ай бұрын
It it available in Hindi or English language
@tushrbanrg67032 ай бұрын
Sitka quarlcrete materials is not good I have used it through their expert over roof