In this video we test the bond-strength of our 4-layer Epoxy Pool Coat system applied on marbelite and fiberglass
These tests were performed to determine the following:
1. To confirm the inter-layer bond-strength between layers applied (24 hours hardening time in-between applications and sanding the hardened layers slightly before over-coating)
2. The overall bond-strength of the epoxy coating to the substrate.
3. The bond-strength of a new coating applied on an old coating after 6 years.
www.poolsolutions.co.za

Пікірлер
BOND-TEST for Concrete ASTM C1583
9:53
Germann Instruments
Рет қаралды 35 М.
Bond Strength Cap Test
2:06
Isolatek International
Рет қаралды 1,5 М.
When You Get Ran Over By A Car...
00:15
Jojo Sim
Рет қаралды 26 МЛН
100❤️
00:19
MY💝No War🤝
Рет қаралды 21 МЛН
КАК ДУМАЕТЕ КТО ВЫЙГРАЕТ😂
00:29
МЯТНАЯ ФАНТА
Рет қаралды 1,2 МЛН
- А что в креме? - Это кАкАооо! #КондитерДети
00:24
Телеканал ПЯТНИЦА
Рет қаралды 6 МЛН
Over-Reinforced Concrete Beam Test
1:33
Structure Pro
Рет қаралды 161 М.
ProShield Epoxy Application Guide
23:05
Pool Solutions
Рет қаралды 1,7 М.
Pull-off Resistance Method for Concrete | James Bond Test | Non-Destructive Testing Methods (NDT) #5
2:11
Fireproofing Pull-test demo
1:41
johnnyo711
Рет қаралды 12 М.
Shear Bond Strength of Dental Bracket Material
0:13
Material Inspection
Рет қаралды 468
Magnifying The World's Brightest Flashlight (200,000 Lumens)
8:55
The Action Lab
Рет қаралды 249 М.
Pre Inspection
7:40
Pool Solutions
Рет қаралды 995
Charpy Impact Test
4:57
MaterialsScience2000
Рет қаралды 1 МЛН
Applying The Primer And Topcoat Epoxy Layers
14:44
Pool Solutions
Рет қаралды 71 М.
Pull off Test, ASTM D4541
2:10
Engineering Civil Integrity
Рет қаралды 2,6 М.
When You Get Ran Over By A Car...
00:15
Jojo Sim
Рет қаралды 26 МЛН