DF-40S Hammer Mill Pulverizer Unboxing & Testing on PCB Components for Gold Recovery. DF-40S Hammer Mill Pulverizer: amzn.to/3SQxtgV Those are affiliate links.
Пікірлер: 22
@ScrappingIrish6 ай бұрын
Interesting, if the chips were incinerated first I would say it would be even better,I have been told that the chips need to be incinerated first before grinding to get the best results, be Interesting to see what way will be best to separate the copper from the plastic after ,love the new machine and video
@timbergdtedt34925 ай бұрын
I'd be interested in a look under the hood if the panels can come off. What ratings are on the motor? Also, it's fine to not freak about getting a damaged shipment. It's not ok to let them get away with it. Extract some insurance or a partial refund. Otherwise, they get sloppier and rougher with everyone's shipment.
@MetalScrapLab5 ай бұрын
I might do the video to show the motor details in the future.
@gevsar66743 ай бұрын
What do you think regarding reliability and longevity? In market lot of for same or less price rock crusher mills for sell. Thanks.
@peteoneill57996 ай бұрын
Be interesting to see how you recover the gold and copper effectively
@craigweller12935 ай бұрын
I've watched this video a few times because I'm looking into the same process for my plated boards rather than just going in to chemicals. Can you show what you do after pulverizing the populated boards. I'm thinking by doing it this way you might get more copper than what it's worth. I like the idea of taking boards down to a powder form and seeing what's next.
@MetalScrapLab5 ай бұрын
I might post a video this week processing about 8 lbs of telecom boards. I'll show all of the process. I have other videos where I'm using blue bowl to separate metals from junk and after that you either take the acids path or cupel or both.
@craigweller12935 ай бұрын
@@MetalScrapLab I figured the blue bowl was part of your process afterwards. The more I was thinking due to how light the plating is, I was afraid it would float and most lost. I'm excited to see your process from start to finish.
@iamthenotbenamed3653 ай бұрын
nice machine brother, for transformers perhaps use Large-Holes, no need have Powder mix, did you try Magnet or Blue-Bowl to Separate, what was Result ...
@MetalScrapLab3 ай бұрын
yeah, the machine is nice, I did use the blue bowl in my other videos, but I'm switching to dry air separation system I'm working on my latest videos.
@iamthenotbenamed3653 ай бұрын
watched most your vids now, very interesting. it seems some nice equipment available from both china and india. We was in midst of starting a LAB with CHEMICALS, yet cant find a SPACE for it. it be loads of Fun following Your-Lead and possibly use ELEC-TRICKERY to take apart MOLTEN-METALS from PCB, unless you can show a simpler way. keep them coming ...
@CdnEwaste4 ай бұрын
Where do you buy this hammer mill?
@MetalScrapLab4 ай бұрын
I got mine from amazon.
@joek5113 ай бұрын
For 1200 bucks , your going to need a whole lot of ICS to pay for that. Several hundred pounds of them
@ekopujimulyono25222 ай бұрын
Berapa Watt???
@josefinagarciatorres47936 ай бұрын
Aora como separa los metales
@Ealdain6 ай бұрын
subsrcibed to your channel i gotta how this works
@user-dn8sg1js5l4 ай бұрын
سلام استاد . قیمت دستگاه چند دلاره متشکرم از راهنمایتون
@MetalScrapLab4 ай бұрын
I paid under $900 from amazon. But they are more expensive maybe about $1200.
@mrgreenswelding28535 ай бұрын
You do need to incinerate the chips first or you wont release the gold from the epoxy
@MetalScrapLab5 ай бұрын
I'm trying to avoid burning anything also I'm trying to move away from acids and replace it with cupel. I do understand what your saying and its a good point but I'm willing to take a slight loss avoiding ashing.