I am depositing a layer of Nickel on a 3D Printed Tree Frog I ordered from JLCPCB with Caswell Electroless Nickel Solution
Пікірлер: 27
@Sapien_by_chanceАй бұрын
Mr Sevilla, that was a very helpful demonstration. Will this electroless nickel plating kit work on polyimide films as well?
@MarvinSevilla-gl2gmАй бұрын
I have not tested on such surface yet
@blake3dcake5 ай бұрын
Amazing results!! Did the coating ever peel or degrade over time? Love the channel btw.
@AngelSevilla-fk6im2 ай бұрын
It was not thick enough to peel. But its nickel so its pretty durable
@heathenxyt8 ай бұрын
Mr. Sevilla, great video! Thank you, however, I'm a little confused about the solutions. You have 2 jugs of the Activator (yellow) and 1 jug of the One-Plate 1 EN solution (green) in the background but in the foreground you seem to have 1 cup of the activator, 1 cup of the "reducer", and 1 cup of the EN solution. What is the "reducer" solution? Is it just the same EN solution?
@nicamarvin8 ай бұрын
Its just Nickel Sulfate as a washing step. You can omit that and just us Distiled water.
@heathenxyt8 ай бұрын
Roger that. Thanks.
@PlatingPulse235 ай бұрын
🔥🔥🔥
@ksrinurepalle82403 күн бұрын
Manku liquid kavali
@olandesevolante64648 ай бұрын
fantastic result! do you supply Caswell products in europe? how can i contact you?
Is the final nickel solution heated? Or can you do at room temperature?
@nicamarvin8 ай бұрын
Unfortunately I have not been able to find room temperature Electroless Nickel solutions that are available to hobbyists. So in all of my videos the Solution is already preheated to close to boiling but it's losing temperature as time goes by, it's good for demonstration purposes, which most of my videos are for.
@jacquescoury29798 ай бұрын
@@nicamarvin so, what my plan was, was to get the room temperature electroless copper kit from caswell to plate all my parts in. Then, the ones that need to be nickel, I was going to purchase the plug n plate wand kit in the nickel/black chrome and then plate using that, since there’s an existing layer of copper already on the part
@nicamarvin8 ай бұрын
@@jacquescoury2979 The Copper layer is too thin. You need to build it thicker.
@jacquescoury29798 ай бұрын
@@nicamarvin could use the Acid copper kit that caswell advertises to use after the electroless copper should you want a thicker layer in that case
@nicamarvin8 ай бұрын
@@jacquescoury2979 Correct.
@charlessarfo43032 ай бұрын
is the nickel room temperature
@nicamarvin2 ай бұрын
No, for 3D prints I lower the temperature to 155(150 being the lowest and 160 the maximum)
@chrisbourlakis1194Ай бұрын
Is that degress or celcius? And what temperature do you head for plastics?
@dominickbadger69152 ай бұрын
Is it conductive?
@AngelSevilla-fk6im2 ай бұрын
Yes, its conductive
@JJ-vp3bdАй бұрын
does this work with bronze?
@MarvinSevilla-gl2gmАй бұрын
Yes
@JJ-vp3bdАй бұрын
@@MarvinSevilla-gl2gm how much does this cost in general if i had a 5 inch tall figure
@electronicsandewastescrapp73843 ай бұрын
I wish they sold the activator in smaller amounts.
@nicamarvin3 ай бұрын
Angel Gilding sells smaller concentrate. angelgilding.com/palladium-sensitizer-concentrate.html I have used their chemicals for more than a decade. But keep in mind that once you mix the palladium concentrate to use it, the shelf life of the mixture is short, You have about 24-48 hours to use it. While the one sold by Caswell Plating is already mixed and has aditives that keep it from going bad.