The Royal Air Mail Service concept vehicle was introduced to the toy market by Meccano in 1935. It cost 6 pence and was sold until 1940. Its futuristic shape for the time was owed to designers who wanted to create a promotion for air mail services in England before war. These models are very rare and hard to obtain today because most of them are falling apart due to their age. The alloy from which they are made cracks and very unpleasant damage occurs. I just received such a car, which I decided to repair using gluing. I proceeded very carefully during the renovation, because any forceful movement could tear off a piece of material. The models were originally packed in 6 pieces in commercial packaging, but I made period packaging based on the Dinky boxes. Thank you for watching the video, I publish car repair videos on Tuesdays and Saturdays. You can turn on subtitles in your language with commentary on the activity in the video.

Пікірлер: 160
@youtellme18
@youtellme18 Ай бұрын
Great to see a toy that kept a child occupied during the horror of war Brought back to life. Well done
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@pajda666chleba
@pajda666chleba Ай бұрын
Piękna renowacja. To aż nieprawdopodobne, że takie autka były w tamtych czasach.
@PaulRestorer
@PaulRestorer Ай бұрын
Dziękuję serdecznie i pozdrawiam
@steppoify
@steppoify Ай бұрын
I am stunned by this Restoration Project. The level of intricate repair prior to primer painting was extensive. But not cripplingly so. The use of Super Glue and Baking soda continues to solve cracked, fragile castings. I have an early Märklin Mercedes racer that is actually crazed all over. The metallurgy of early alloy castings was problematic and evolving. Maestro, finishing all the filing, bodywork, and putty work was amazing to watch. A new process has been added. Using a drill to spin the rims to apply the Molotow chrome. The finished piece is lovely. A beautiful job. ❤ The original white tires were toy tires. The tires here match the actual original Royal Airmail tires. Lastly, the nicest graphically conceived box art I've seen. Kudos and Congratulations, Pawel. A job VERY well done! Best, Stephen😊
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Stephen
@MKminiaturecarremodelingStudio
@MKminiaturecarremodelingStudio Ай бұрын
I am always amazed by the wonderful restorations. Paul, when I watch your channel, I naturally learn about the history of miniature cars!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@chrissharp5073
@chrissharp5073 Ай бұрын
Another classic model saved from the scrapyard, well done. The hard work has paid off.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@bubygorgocoleccionablesarg8368
@bubygorgocoleccionablesarg8368 Ай бұрын
Fantastic work, beautiful model, congratulations!!
@geo2cv6tron14
@geo2cv6tron14 Ай бұрын
The advantage of your videos is that, not only do I admire the quality of your restorations, but it also makes me discover cars like this one that I didn't even know existed, which adds to the usefulness pleasantly 🤩👍
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@ThePerfectSeason1972
@ThePerfectSeason1972 Ай бұрын
Incredible Magical Restoration - right before one’s own eyes. I like the way you make the boxes and how you scoot the car into it!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@BulletNoseBetty
@BulletNoseBetty Ай бұрын
What a terrific restoration! Let's not forget that car is *89* years old! Great job!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@rosemorrison7075
@rosemorrison7075 Ай бұрын
Hi Paul. Absolutely incredibe restoration of such a damaged little vehicle. Your patience and attention to getting it back to correct proportions and specifications is appreciated. Thanks for showing us this most unusual and interesting little car.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@rjung_ch
@rjung_ch Ай бұрын
I have never seen such a vehicle ever, so very strange proportions. But you made it new again. Thanks Paul 👍💪✌
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@PirataDesign
@PirataDesign Ай бұрын
Questa volta hai salvato un vero reperto storico.... Ha quasi 90 anni questo modello e devo dire che è anche fatto molto bene per le tecniche dell' epoca . Chissà in quanti hanno giocato con lui e chissà quante mani ha passato per arrivare ai giorni nostri in condizioni abbastanza discrete. E come sempre l' hai restaurato alla perfezione e ne hai valorizzato gli aspetti più significativi. Tanti tanti tanti Complimenti!
@PaulRestorer
@PaulRestorer Ай бұрын
Grazie mile Pirata
@mohammedkhaliedrafsan3547
@mohammedkhaliedrafsan3547 Ай бұрын
Very Wonderful Renovation Paul ❤️🇧🇩🥰🇧🇩❤️
@murielbecel5328
@murielbecel5328 Ай бұрын
Bonjour Paul beaucoup de travail mais parfait 👍👍😍😍
@martindaredare
@martindaredare Ай бұрын
Very smart restoration of this very old early dinky toys ,not easy when it's full of cracks. All the best Martin
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Martin
@shanethompson2915
@shanethompson2915 Ай бұрын
Fantastic result for an old wreck.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@Willshit71
@Willshit71 Ай бұрын
Awesome 🎉 restoration on this diecast vehicle Paul!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@mikhaelshushanyan
@mikhaelshushanyan Ай бұрын
Me personally wait for the moment when Paul cuts the box out of the print, folds it, puts the model into the box, rotates it to the side and lets the viewer feel that moment of satisfaction for a second or two. Awesome!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@NLKINK
@NLKINK Ай бұрын
Outstanding Paul. A thorough restoration with a few extras. This battered little trooper found a new home!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@BlackCat-nv5sf
@BlackCat-nv5sf Ай бұрын
Beautiful resto are usual Paul. Great to see such an old casting be restored for current generations to see and enjoy.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@diecast_MikeEspo
@diecast_MikeEspo Ай бұрын
Awesome casting . This one was bad considering what we have seen you restore. Great finish, full watch and share. NICE 👍 Mike .
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Mike
@billwashburn8568
@billwashburn8568 Ай бұрын
Nice, I do like the boxes a lot. I appreciate the work that goes into such a small project. Well done sir.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@markrigg7038
@markrigg7038 Ай бұрын
Lovely model, looks like a plane as well, superb restoration Paul 👍👍
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Mark
@randytaylor1258
@randytaylor1258 Ай бұрын
Wow! That's a work of art, Paul. Cheers!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@brianartillery
@brianartillery Ай бұрын
I have heard of this model - because of it's fragility - down to metal fatigue, like a lot of Dinky's pre, and immediate post war models - it's legendary in it's scarcity. I have never seen a real example, and so your video is a real treat. Lovely work, to create such a beautiful restoration. Thank you.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@pavelkoudele5526
@pavelkoudele5526 Ай бұрын
Z ošklivého kačátka se zrodila krásná labuť. Díky. Pavel 🇨🇿
@joeholloway1386
@joeholloway1386 Ай бұрын
Nice restoration, details and paint job 👌 👍
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Joe
@BelgianDiecastRestorations
@BelgianDiecastRestorations Ай бұрын
Very impressive work! Especially the filling of the cracks on the body.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@ernestoclaudodip9671
@ernestoclaudodip9671 Ай бұрын
Hello Paul , you made a delicate hard work with this old car. Congratulations.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@moedasmais
@moedasmais Ай бұрын
Ficou muito bonito Paul, parabéns! 👏👏👏👍
@septiccalling8341
@septiccalling8341 Ай бұрын
Outstanding! That's a great 'save' of a .....what? Nearly 90 year old toy. Excellent! 👍🏻👌🏻👏🏻
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@whistlingdiesel
@whistlingdiesel Ай бұрын
What an interesting car, a '34 Duple Coachbuilders body on a Morris Commercial chassis.
@austingreenough6396
@austingreenough6396 Ай бұрын
Well done Paul,You have a great survivor model now. Enjoyed your video Austin
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Austin
@jamescasey240
@jamescasey240 Ай бұрын
Wonderful resto! That blue paint colour is magnificent!
@briansdiecastthailandstoth6747
@briansdiecastthailandstoth6747 Ай бұрын
That is a very cool old Dinky ...Nice work Paul......
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Brian
@carlosalbertobouza5573
@carlosalbertobouza5573 Ай бұрын
Muy bueno Paul...!! Gracias por compartir.. Un abrazo desde Argentina
@PaulRestorer
@PaulRestorer Ай бұрын
Muchas gracias
@frasermartin6728
@frasermartin6728 Ай бұрын
Exemplary lesson: i never seem to be able to get the superglue and baking soda to work strongly enough to reshape it, but it seems a tortoise pace, rather than a hare's, is the winning combination. Great rescue of a rare beast!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Martin
@joramamodellbau3987
@joramamodellbau3987 Ай бұрын
Exzellent. mit diesem tollen Ergebnis hast Du dem Dienstwagen der Royal Air Mail zu einem neuen Leben verholfen. Eine mehr als sehenswerte Arbeit, Paul. Gruß, Joachim Doskonały. Tym wspaniałym wynikiem dałeś nowe życie służbowemu samochodowi Royal Air Mail. Dzieło więcej niż warte zobaczenia, Paul. Pozdrawiam, Joachim
@PaulRestorer
@PaulRestorer Ай бұрын
Vielen Dank Joachim
@peterkress4592
@peterkress4592 Ай бұрын
Perfekt Paul 👍💯🌎🇩🇪
@daniloweifu9566
@daniloweifu9566 Ай бұрын
Ich finde den echt cool. 🤠🤘
@PaulRestorer
@PaulRestorer Ай бұрын
Vielen Dank Peter
@daniloweifu9566
@daniloweifu9566 Ай бұрын
@@PaulRestorer Peter no Danilo yes
@FelloniusWizard
@FelloniusWizard Ай бұрын
What a classic! Neat job!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@teebodk3917
@teebodk3917 Ай бұрын
Wow, what a project... like restoring an eggshell! I'm amazed that it didn't fall completely apart. A restoration like this is extremely valuable since, as you say, there are so few left, and even when stored under optimal conditions and handled with extreme care, the number of survivors will continue to diminish as more and more disintegrate, meaning that the earliest parts of Dinky history risk being lost. I wonder if your applications of glue, primer and paint could possibly cause further degradation processes of the metal, only time will tell, and I assume you'll be keeping a watchful eye on it in the future.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@marekm2561
@marekm2561 Ай бұрын
Dzięki Pawle! Pozdrawiam! 👽🖖
@PaulRestorer
@PaulRestorer Ай бұрын
Dziękuję serdecznie
@Geniuz.Studio
@Geniuz.Studio Ай бұрын
A to niespodzianka. Wow!
@PaulRestorer
@PaulRestorer 7 күн бұрын
Dzięki
@stevenjones19-m8i
@stevenjones19-m8i Ай бұрын
Hello Paul, another great model,these being metal from the old corgi they seem quite easy to restore.
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Steven
@that_thing_I_do
@that_thing_I_do Ай бұрын
What a cute looking car!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@srocarg
@srocarg Ай бұрын
i love this models are beautiful
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@andreasschweminski6808
@andreasschweminski6808 Ай бұрын
Wow alle Achtung lieber Paul, diesmal hast dich auf ein sehr schwieriges Modell eingelassen aber mit Bravour ein tolles Modell heraus bekommen 😊gratuliere dir zum schönen Erfolg. Mfg aus Hamburg
@PaulRestorer
@PaulRestorer Ай бұрын
Vielen Dank Andreas
@janbotha571
@janbotha571 Ай бұрын
Perfect Paul 🎉💯🤗😎☕
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Jan
@ananndavinci
@ananndavinci Ай бұрын
Awesome.... White rubber tyres would have made it look more stock Dinky. 😌 🙏 Live Long N Prosper
@steppoify
@steppoify Ай бұрын
@@ananndavinci The car with Navy hubs and black tires looks like the actual car. I feel the point here was to make it more a truthful scale model rather than a "toy." The chrome application on the roof and fin were also original to the real car.
@luizcarlosdias3690
@luizcarlosdias3690 Ай бұрын
Pail, mais uma bela restauração. Gostei da criatividade na pintura das rodas. E uma dúvida, sei que o modelo era azul e voce seguiu isso, mas a cor do Royal Air Mail é vermelho, será que em 1935 era azul? Parabéns.
@sebastianolivera6005
@sebastianolivera6005 Ай бұрын
Exelente Paul, saludos desde Argentina!!
@PaulRestorer
@PaulRestorer Ай бұрын
Muchas gracias
@Collectorholic
@Collectorholic Ай бұрын
Nice and shiny!
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@te-cto
@te-cto Ай бұрын
Super 👍 👍👍
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@alessandroalberto6431
@alessandroalberto6431 Ай бұрын
Very nice !
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@paulpisters668
@paulpisters668 Ай бұрын
Imagine a world without super glue. 😅
@martinbalmforth2665
@martinbalmforth2665 Ай бұрын
Hey Paul, I always put a lint free cloth down when reassembling models after paint to cut the risk of scratches. Nice work as usual
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@theartoftimelapsemore424
@theartoftimelapsemore424 Ай бұрын
This is a real car from 1934. It's a 1934 Morris-Commercial 15 cwt Royal Mail Air Service Car Duple [L2].
@PaulRestorer
@PaulRestorer Ай бұрын
cool
@enricoorsettopavan9892
@enricoorsettopavan9892 Ай бұрын
Esemplare Splendido 😻🏆 ♻️ ⭐⭐⭐⭐⭐ Grazie Paul💪💪💪🫶👍 Ottimo Recupero
@PaulRestorer
@PaulRestorer Ай бұрын
Grazie mile
@jeanlucmartinez4340
@jeanlucmartinez4340 Ай бұрын
Bonjour Paul. Merci pour cette nouvelle vidéo. J'aimerai savoir quelle pression et quelle dimension d'aiguille tu utilises quand tu peins ces petites voitures à l'aérographe ? Je débute à l'aérographe et je ne trouve pas ces informations sur le net sauf pour les figurines. Merci
@Romanek1981
@Romanek1981 Ай бұрын
Kolejna bardzo dobra robota 👏😁
@PaulRestorer
@PaulRestorer Ай бұрын
Dziękuję serdecznie i pozdrawiam
@ukaszmianowski4176
@ukaszmianowski4176 Ай бұрын
👍👍👍🦄
@PaulRestorer
@PaulRestorer Ай бұрын
Dziękuję bardzo
@Bikelife9883
@Bikelife9883 6 күн бұрын
Great restoration of an old model that was literally starting to crumble. I appreciate this might sound a bit 'nit picky', but the car is from the 1930's and the door decal has a 'Queen's crown'. It should be a 'King's crown' which is a different shape. Still a great job, keep up the good work.
@PaulRestorer
@PaulRestorer 5 күн бұрын
Thank you very much
@fredburley9512
@fredburley9512 Ай бұрын
Beautiful toy but I think the white walled tyres would of set it off. Lovely job as usual. 👍
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@mohammedkhaliedrafsan3547
@mohammedkhaliedrafsan3547 Ай бұрын
My Name Is Mohammed Khalid Rafsan I Living In Pallabi Mirpur Dhaka Bangladesh My Gender Was Male I Watched Your Renovation Video 🥰🇧🇩🥰
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much Mohamed
@michaelmarcotti2470
@michaelmarcotti2470 Ай бұрын
Looks like a Tatra.
@PaulRestorer
@PaulRestorer Ай бұрын
Yes of course
@kir_kras
@kir_kras Ай бұрын
О, да! Восстанавливать огрехи литья металла - это, выражаясь по-русски, жопа! Но ты справился! Всё у тебя нормально получается👍👍👍
@PaulRestorer
@PaulRestorer Ай бұрын
Большое спасибо
@user-qq6ye6pq7p
@user-qq6ye6pq7p Ай бұрын
🔥👍😎🇺🇿
@paul-sparky-sparr4160
@paul-sparky-sparr4160 Ай бұрын
10 o'clock postman... 🎶🎵 🤣 Cóż... jakoś mam tę piosenkę w głowie. Bardzo niezwykła renowacja. (Jeśli dobrze zrozumiałem, trzeba było przerobić ciało 7 razy 😳) Wysiłek się opłacił, a efekt jest fenomenalny 🤩👍🏼 Stara biżuteria znów lśni nowym blaskiem, a wisienką na torcie jest autentycznie wyglądające „oryginalne opakowanie”. Brawo Paweł, jestem zachwycony. Oczywiście, dwa kciuki w górę 👍🏼 👍🏼 Dziękuję za udostępnienie 🙏🏼 i tak trzymaj przyjacielu 😉 Życzę miłego tygodnia Tobie i Twojej rodzinie, bądźcie zdrowi i pogodni. Pozdrowienia ze słonecznego Morza Północnego ☀️🌊🏄🏽‍♀️🏖️ 👍🏼🇵🇱😎🍻🤠🇩🇪👍🏼 10 o'clock postman... 🎶🎵 🤣 Well... somehow I have the song in my head. A very extraordinary resto. (If I understood correctly, you had to rework the body 7 times 😳) The effort was worth it and the result is phenomenal 🤩👍🏼 An old piece of jewelry shines again in new splendor. And the authentic-looking "original packaging" is the icing on the cake. Good onya Paul, I'm thrilled. Clearly, both thumbs up for that 👍🏼 👍🏼 Thanks a lot for sharing 🙏🏼 and keep it up,mate 😉 Have a nice week to you and your family and stay safe and sound. Greetings from the sunny North Sea shore ☀️🌊🏄🏽‍♀️🏖️ 👍🏼🇵🇱😎🍻🤠🇩🇪👍🏼 10 o'clock postman... 🎶🎵 🤣 Naja... irgendwie hab ich das Lied im Kopf. Eine ganz außergewöhnliche Restaurierung. (Wenn ich das richtig verstanden hab, mußtest du die Karosserie 7x überarbeiten 😳) Die Mühe hat sich gelohnt und das Ergebnis ist phänomenal 🤩👍🏼 Ein altes Schmuckstück erstrahlt wieder im neuen Glanz.Und Die authentisch wirkende "Originalverpackung" ist das Tüpfelchen auf dem I. Gut gemacht, Paul, ich bin begeistert. Ganz klar, beide Daumen hoch dafür 👍🏼 👍🏼 Vielen Dank fürs teilen 🙏🏼 und mach weiter so, mein Freund 😉 Dir und Deiner Familie noch eine schöne Woche und bleibt gesund und munter. Gruß von der sonnigen Nordsee ☀️🌊🏄🏽‍♀️🏖️ 👍🏼🇵🇱😎🍻🤠🇩🇪👍🏼
@PaulRestorer
@PaulRestorer Ай бұрын
Vielen Dank Paul
@leonardoserra1386
@leonardoserra1386 Ай бұрын
Lindo malavioso Cesasomal top ❤❤❤❤❤
@PaulRestorer
@PaulRestorer Ай бұрын
Muito obrigado Leonardo
@typhoon9454
@typhoon9454 Ай бұрын
Just Great!...
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@carmium
@carmium Ай бұрын
~3:30 you say "remove the old paint in baking soda" when you mean *caustic* soda. Big difference!
@PaulRestorer
@PaulRestorer 5 күн бұрын
the translator must have made a mistake. Sorry about the artificial intelligence
@danieldusek9454
@danieldusek9454 Ай бұрын
Pěkná práce, mám jen dvě výhrady. Proč nejsou pneu bílé a znak na dveřích barevný?
@garagemslzv8465
@garagemslzv8465 Ай бұрын
Tops
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@billchisholm7334
@billchisholm7334 Ай бұрын
Great job Paul, what is the white powder you use with the glue? I have meant to ask for a while. Thanks
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@modellbahnagenda
@modellbahnagenda Ай бұрын
Kompliment 👍👍👍
@PaulRestorer
@PaulRestorer Ай бұрын
Vielen Dank Uwe
@euzebi7512
@euzebi7512 Ай бұрын
0:54 No i zepsułeś ... jak to mówią "chciałem dobrze a wyszło jak zwykle" 🙂 (czyż życie nie jest dziwką?) 😋
@PaulRestorer
@PaulRestorer Ай бұрын
no niestety nieraz się nie uda
@dankamosna2870
@dankamosna2870 Ай бұрын
Paul, preco si na zafixovanie kolies nepouzil priklep a svoj nastroj na rozklepanie osky???😮 vysledok by bol o 100 % lepsi ...
@PaulRestorer
@PaulRestorer 5 күн бұрын
Bohužiaľ, v tomto prípade jeden zásah kladivom spôsobí, že sa celý prvok rozpadne
@MisterGames
@MisterGames Ай бұрын
Almost 100k. C'mon
@neilhaas
@neilhaas Ай бұрын
🇨🇦🇨🇦🇨🇦🇨🇦💯❤️🤩😊
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@evan_kumar
@evan_kumar Ай бұрын
14:16 I heard your stomach growling!
@user-ql9op5qr5o
@user-ql9op5qr5o Ай бұрын
As rodas com esse acabamento fica uma porcaria
@onerege
@onerege Ай бұрын
Nice restoration, but this car is 89 years old! Why should we destroy the original and Should and add glass?
@MsMarcow
@MsMarcow Ай бұрын
A rather creative restoration. There isn't much left of the model's original appearance here
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much
@daniloweifu9566
@daniloweifu9566 Ай бұрын
Das Auto ist hässlich aber deine Arbeit ist fantastisch. ❤🤠🤘 Grüße aus Deutschland, Mecklenburg-Vorpommern.
@PaulRestorer
@PaulRestorer Ай бұрын
Vielen Dank
@MetalMania3DTV-TAS-AUS
@MetalMania3DTV-TAS-AUS Ай бұрын
Absolutely magic restoration Paul on such a bad casting 👌🍻🍻🇦🇺🇦🇺🤝🦘🏔🌧🌨❄️
@PaulRestorer
@PaulRestorer Ай бұрын
Thank you very much KC
@Classic70s80s90s
@Classic70s80s90s Ай бұрын
Prabéns Meu Amigo ! Restauração Como Sempre Perfeita
@PaulRestorer
@PaulRestorer Ай бұрын
Muito obrigado
Jumping off balcony pulls her tooth! 🫣🦷
01:00
Justin Flom
Рет қаралды 29 МЛН
Я обещал подарить ему самокат!
01:00
Vlad Samokatchik
Рет қаралды 9 МЛН
Useful gadget for styling hair 🤩💖 #gadgets #hairstyle
00:20
FLIP FLOP Hacks
Рет қаралды 11 МЛН
[Build diary #04 Final] - 1/24 Tamiya Porsche 934 Jägermeister
25:45
José Diego Quignon Terrada
Рет қаралды 86
Weathered Freightliner Truck scale 1:24 from ITALERI
32:45
Laser Creation-World
Рет қаралды 288 М.
Dinky restoration of Volvo 1800 S No. 116 Toy model cast.
29:36
Paul Restorer
Рет қаралды 16 М.
Build Metal Tank T-34 | How to make a tank from an oven | homemade RC Tank
12:28
Поймал ГНУСНОГО и ПОДЛОГО перекупа.
0:42
Саша Туман
Рет қаралды 1,6 МЛН
ИНТЕРЕСНАЯ ПОКРАСКА АВТО
0:17
Films
Рет қаралды 2,5 МЛН
@nastya_adaeva_ #рек #automobile #авто #авария #машина #топ #ремонт
0:29
T55 Narxi 23 900$ 📞95 155 03 00 | 📞91 033 03 03
0:18
China Avtouz
Рет қаралды 8 МЛН