The toggle is not in locked position when the mold is closed.
@sampleoffers1978Ай бұрын
Heat storing polymers should end the over reliance on precious metals for electric vehicles. Main thing cobalt does is heat up quickly.
@Study-bz6kjАй бұрын
How to solve the problem of condensation?
@KruseTrainingАй бұрын
Condensation can occur if the mold temperature and molding room humidity are not balanced. You must analyze and reduce the level of humidity in the room.
@renrut02 ай бұрын
this is not difficult to do........do extrusion or injection blow molding....like a bottle.......done it, this is very simple molding
@kalpeshparikh19072 ай бұрын
Any tutorials
@KruseTraining2 ай бұрын
www.krusetraining.com our eLearning website
@unidentifiedhandle6 ай бұрын
Great video, it would have been perfect if example was shown to fully understand the final results! Thanks!
@KruseTraining3 ай бұрын
Great point!
@user-wz5tq6to4u6 ай бұрын
In your opinion, is a high contour cashew gate suitable for use with 30% glass filled PBT?
@KruseTraining3 ай бұрын
The design and size of the gate are the most important aspects to decide if it is suitable for your material. The process will also determine the cashew gate's flexibility to be properly ejected.
@ritafong85877 ай бұрын
One of the best videos! Thanks.
@sreeragramakrishnan66837 ай бұрын
Where can I get the full video?
@pawanraghav51788 ай бұрын
thanks, useful!
@chelseykamron41438 ай бұрын
'promosm' 🌺
@HemangJoshi9 ай бұрын
Any docs links?
@allanguimaraes Жыл бұрын
Great!
@naveenkushwaha6305 Жыл бұрын
Respected Sir, Could you tell me on which software you're running this analysis?
@KruseTraining Жыл бұрын
We used Moldex3D software to run these simulations.
@user-yy6ji6wn8p Жыл бұрын
😝😝😝😝😝😋😛😜🤪🤑🫠 Bravo 🎶 Bravo products Bravo fans
@nickysmolenaers9316 Жыл бұрын
Where can I buy this ?
@KruseTraining3 ай бұрын
Our eLearning is available at www.krusetraining.com
@bhilapatil939 Жыл бұрын
Is support and service available at India?
@KruseTraining3 ай бұрын
Not yet
@amjadmahmoodmirza763 Жыл бұрын
Good information
@jamieevans6395 Жыл бұрын
You get this a lot with abs if you're injecting onto a flat surface hence why you should inject onto a wall of the component
@Learn_123 Жыл бұрын
Very informative content plz keep posting this kind of content thanks lot
@miniosis1457 Жыл бұрын
Plzz reply a humble request
@miniosis1457 Жыл бұрын
Can u teach me
@miniosis1457 Жыл бұрын
Hi sir
@FratDede Жыл бұрын
So what is your recommendations?
@jamieevans6395 Жыл бұрын
You will have to profile the first stage to try and control it and putting tool temps up will help
@ezyplast2 жыл бұрын
Niceuo
@pro-plastics9082 жыл бұрын
very interesting, does it the simulation actually translate when molding actual parts.
@KruseTraining2 жыл бұрын
Simulation is very effective in identifying key process variables and to minimize process development time for a new tool.
@carlosluis67812 жыл бұрын
Thank you for sharing this information.
@alexanderravi49692 жыл бұрын
I'm first viewer from india 😀
@susanvaaler79762 жыл бұрын
Great job Torsten! I love how you narrate this because it makes it so understandable. Keep up the great work!
@KruseTraining2 жыл бұрын
Thank you for the positive feedback, Susan!
@alexanderravi49692 жыл бұрын
Pls make videos on troubleshooting
@mahmoudradwan29792 жыл бұрын
👍
@designmaking96042 жыл бұрын
Nice
@Anilkumar-sq4tp2 жыл бұрын
Sir, 1) What's the Best way to take bearing. 2) How to reduce bearing time of mold. 3) In what way we can maintain and design to reduce bearing time . 4) how to use tolerance for mfg of mold. Kindly Can you make a video for the same with good and tough mold as example.
@minhkhanh23932 жыл бұрын
Best Channel
@minhkhanh23932 жыл бұрын
Best Channel !
@quazi.shahin2 жыл бұрын
thanks for sharing👍
@3Dscanhouse3 жыл бұрын
Is there is a full training course material to buy ?
@KruseTraining3 жыл бұрын
Yes, you can purchase a subscription to our full training program here: krusetraining.com/subscribe/ or purchase individual lessons here: krusetraining.com/lesson/
@Anilkumar-sq4tp3 жыл бұрын
Excellent Stuff, Presentation. Job well done. What software you normally prefer for mold flow analysis and cooling analysis ? I use UG NX and Creo as well. I do mold flow analysis, for injection molding. Thank you. looking for ward.
@KruseTraining3 жыл бұрын
We use Moldex3D (www.moldex3D.com) software for mold flow, cooling, shrinkage and warpage analyses.
@Anilkumar-sq4tp3 жыл бұрын
@@KruseTraining thanks for quick response and reply. Keep it up. I have few tough questions to you. Looking forward. Keep it up good work. Have a great day.
@ricardooliveira2883 жыл бұрын
perfect learning with video and simulations. Perfect.
@diaaeldinismail64963 жыл бұрын
We need more videos please
@arafatalgazaly34893 жыл бұрын
Very good video . I really appreciate your great effort
@allaboutmould22523 жыл бұрын
Runner length should be small as much as possible
@ricardooliveira2883 жыл бұрын
very good. the training didactics are great showing the application directly in the software. They are to be congratulated. pity that the dollar in Brazil is practically 1 to 6. when I reduced that absurd difference, I intended to acquire this training.👏👏👏👏
@juanjosevillegas94453 жыл бұрын
Excelente AND cobrar presentación
@ezyplast4 жыл бұрын
Love this channel
@subhasharkasali29844 жыл бұрын
The concept of the subject of gates visualization is quite educative.
@surajprakash32644 жыл бұрын
Hello Sir, I have a question to you: If we are creating a two cavity or multi-cavity mold, how do we decide how much distance should be kept between two cavities? Because its directly related to the runner length.
@KruseTraining4 жыл бұрын
Cavity distances are dependent on part design and gating options. If no side actions are required to relieve undercuts, the cavity distances can be small, minimizing the cold runner length and material waste. The same is true when using hot runners. Every new product design should be evaluated based on tool functionality. For more detailed information please subscribe to www.krusetraining.com
@surajprakash32644 жыл бұрын
Hello sir can you explain what does mean of material shearing ??
@KruseTraining4 жыл бұрын
When plastic material enters a mold it exhibits "fountain flow behavior" - similar to a water fountain. The material immediately cools on the mold wall, creating a difference in flow velocity. This effect results in shear differences in the flowing layer of the material. Please subscribe to www.krusetraining.com for a more detailed explanation.