Hey bro listen after I added SMB it precipitated gold, but the solution still has gold in it. How do I get the rest out?
@PoorMiners32159 минут бұрын
Do you neutralize nitric? If not then its imposible to get gold out from solution, contenue add smb until foaming comes on the top of solution, then add distilled water to dilute solution.
@andrebattis941016 минут бұрын
Yeah I did with sulfamic acid. But after I add smb first I get gold not all of it though. My stanneous is still positive. So do I know add hcl and heat it to add sulfamic then smb again. Right ...
@nativeflight707920 сағат бұрын
What do you do with the slime after?
@PoorMiners32158 минут бұрын
I roast it then chlorine leach.
@JayboyBerces-kw3wu22 сағат бұрын
Sir Meron Po akong ganian Marami po
@PoorMiners32158 минут бұрын
Sigi durogin mo at e panning
@jessavaldez4678Күн бұрын
boss pwede mag try nang bato magkano bayad..baka maylaman.
@PoorMiners32157 минут бұрын
Bro hindi po pwedi, nasa malayo po ako, ikaw na mag try.
@user-qg8gd9sq4c2 күн бұрын
❤❤❤
@user-fl9ih9dy9y3 күн бұрын
Boss pag pinakuluan walang muriatic na i dadagdag sa tubig.o mayron pa
@PoorMiners3213 күн бұрын
Sa paghuhugas ba ibig mong sabihin? Kung sa paghuhugas na e wala ng muriatic yun
@user-fl9ih9dy9y2 күн бұрын
@@PoorMiners321 diba pagkatapos mo tanggalan ng maraming tubig pinakuluan mo naman sa tubig peru diko nakita sa vidio na nilagyan mo ng muriatic pero sa ibang vlog mo nilagyan mo ng muriatic at tubig bago mo pakuluan salamat
@PoorMiners3212 күн бұрын
Oo yan kasi ang tamang paraan, kasi ang sabi ko doon, sundin nyo lang ang video tungkol sa washing na ginawa ko bro
@user-ld6og5xl3w3 күн бұрын
سلام این سنگها در هر کیلو چقدر طلا میشه استخراج کرد
@PoorMiners3213 күн бұрын
300grams per ton brother.
@atNguyenVan-qx3ex3 күн бұрын
0:17
@user-fl9ih9dy9y3 күн бұрын
Boss paano ba gumawa ng stanous cloride.pinapakuloan ba ng matagal ang tingga sa muriatic
@PoorMiners3213 күн бұрын
Bro yung tingga na sinasabi mo hindi yan pwedi gawing stannous test kasi lead man yun, yung ginagamit sa stannous test ay pure tin metal. Ibabad mon lang yung tin sa muriatic hanggang matunaw lahat ratio nito ay 15grams of pure tin, 50ml muriatic.
@user-fl9ih9dy9y3 күн бұрын
@@PoorMiners321 boss yung ginagamit sa pang shouldering sa celphone at tv.na lead...yung naka ruliyo...siya
@PoorMiners3213 күн бұрын
Yung ibang soldering wire mataas yung content ng lead maghanap ka ng mataas ang contain ng tin,
@cafenatedfox11894 күн бұрын
Can u make a video on how to use sodium thiosulfate for gold leaching? I'm curious if it will work as good as sodium cyanide
@PoorMiners3213 күн бұрын
Soon brother..
@CamRStanford4 күн бұрын
Sulfamic acid will neutralize excess nitric acid, and it will precipitate lead as lead sulfate at the same time as the sulphamic acid is oxidized into sulfiuric acid.
@PoorMiners3214 күн бұрын
Thanks
@PoorMiners3214 күн бұрын
Thanks
@msaric12064 күн бұрын
i am a photografer.
@PoorMiners3214 күн бұрын
Nice
@shucksful4 күн бұрын
Why did it take so long to turn purple? It’s usually a much quicker reaction considering how dark the purple is. Was there water in your syringe.
@PoorMiners3214 күн бұрын
That's the reaction of low gold contain in aqua regia solution sample brother..
@abeleski4 күн бұрын
Take care of yourself. Stay healthy
@PoorMiners3214 күн бұрын
Thank you very much brother
@abeleski4 күн бұрын
Take care of yourself. Stay healthy
@PoorMiners3214 күн бұрын
Thanks
@navrangstudio82734 күн бұрын
Dear sir how mach gold in one camera
@PoorMiners3214 күн бұрын
That is few amount of gold brother
@msaric12064 күн бұрын
and there is a gold or silver in film emulsion
@PoorMiners3214 күн бұрын
Maybe nothing brother
@shineyrocks3905 күн бұрын
Save that lens from that camera. It will make a nice jeweler's loop to see micro gold in ore. 😊
@PoorMiners3215 күн бұрын
Thank you yes sir, nice lens..
@user-fl9ih9dy9y5 күн бұрын
@@PoorMiners321boss tinunaw ko sa muriatic acid at hydroge peroxide ang gold foil ko na subra 50 grams na nakukuha ko sa mga celphone pins at mga computer at mga loptop...mga ilang gram kaya na makukuha ko duon na ginto
@ukskywatcher95985 күн бұрын
👍🙏
@ciffenwealth6 күн бұрын
what a nice button of gold, perfect mining. that's the same in Phelix Mining area before but just imagine the company, its operational until now.. so does around and nearby of this Benguet.. your new subscriber watching many times @CIFFEN..
@PoorMiners3215 күн бұрын
Thank you bro..
@YourDailyVideoNews6 күн бұрын
Excellent Forge 👍👍👍
@PoorMiners3216 күн бұрын
Thanks
@YourDailyVideoNews6 күн бұрын
Excellent test, Brother 🙏🙏
@PoorMiners3216 күн бұрын
Thanks brother
@benmartin57146 күн бұрын
Thanks, I wondered how this was done.
@PoorMiners3216 күн бұрын
Thanks, very simple brother..
@mihaiilie88087 күн бұрын
You will be the best on youtube when you do the thiosulfate video.
@PoorMiners3217 күн бұрын
Yes sir but so far my 2 trials attempt wasn't successfull, very difficult to handle the pH.
@mihaiilie88086 күн бұрын
@@PoorMiners321 Another good one for you is gold flotation. Flotation plus panning is more efficient than cyanide and better if there is carbon or gold sulphides.
@mihaiilie88085 күн бұрын
@@PoorMiners321You should switch to gold flotation then. And since you wont have Xanthates, i reccomend Dithiocarbamate ( found as fungicide) instead of Xanthate- and works better. Flotation plus gravity separation, is better than cyanidation in most cases.
@user-jk6cp6rz4i8 күн бұрын
Золото видит нас 😅
@PoorMiners3218 күн бұрын
Kita gid sa imung dakung mata.
@andrebattis94108 күн бұрын
Hey bro listen I messed I think. I had a 3 gallons of aqua regia I add ferrous sulfate to it. But it seemed like it didn't work so I used a little lye. And cemented iron and other. I took brown sludge added HCL and turned green. But there's grey sludge at the bottom it takes forever to strain. Do you think if I added aqua regia to the sludge I can get back my gold. Sorry I don't else to ask and your really good at this I would appreciate it. Thanks
@PoorMiners3218 күн бұрын
3 gallons of aqua regia? What are your gold source? From electronics? Or from gold ore? But anyway, when you add iron sulfate you need to stir longer, allow the gold to precipitate, be patience, the problem here you add lye, lye can precipitate all metals, now this time you started to add lye then continue the job by adding lye to completely precipitate all metals then filter, then boil with distelled water multiple times until no more lye then dissolve the precipitate again with hno3 with distelled water 50/50 in ratio then the remaining resedue dissolve to aqua regia.
@andrebattis94107 күн бұрын
I took the white sludge that was in the bottom tested it and it came back a little that it was gold. It was was so hard to strain, but then I dissolved it in aqua regia and that's where I'm at now
@hashemameli36669 күн бұрын
excellent. I am proud of you for carefully explaining all the important issues of gold bearing stones. Or you explain that when there is gold and mercury in the stone, the color of the complex becomes reddish brown. You are the best in the gold group. For easier extraction, I add a solution of copper nitrate or copper chloride to a stone that contains only gold and wash it at high heat. Ionic gold is alloyed with copper and can be separated in larger sizes. good luck. Hashem Ameli
@PoorMiners3219 күн бұрын
Thank you very much brother..
@user-pu3oo6de4i10 күн бұрын
رائع وهل تتعامل بالزئبق ام بالماء الملكي أو بفرن الصهر
@PoorMiners32110 күн бұрын
شكرا لك أخي سأستخدم الزئبق عندما أعتقد أن درجة نقاء الذهب المجهري عالية وليس الذهب المعقد، وسأستخدم أيضا الماء الملكي للذهب الذي يأتي من الصخر كون درجة نقاء الذهب المجهري عالية وليس ذهبا معقد، ليس لدي فرن حتى الآن يا أخي، ولكن هذا هو حلمي الأكبر، في يوم من الأيام عندما أكسب المال وأستطيع توفير المال للشراء قريبًا
@24KGOLDRECOVERY10 күн бұрын
Excellent 🎉
@PoorMiners32110 күн бұрын
Thanks
@user-fl9ih9dy9y10 күн бұрын
Boss yung clorine puwedi pala irecover ng gold foil.kasu sinubukan ko nayan hindi ko narecover ang ginto sa gold foil napagud lang ako sa kakaipon ng mga gold plated pins nasayang lang parang humalo lang ata sa muriatic acid
@PoorMiners32110 күн бұрын
Baka naramihan mo sa pag lagay ng chlorine boss, wag mo itapon ang solutions mo e babad mo sa init ng araw, hayaang nakabus mga dalawang araw tapos e filter mo tapos precipitate mo gamit ang iron sulfate
@andrebattis941010 күн бұрын
What temp do you have to have to add sodium hydroxide. Good job
@PoorMiners32110 күн бұрын
Room temperature only. Because sodium hydroxide create already heat during addition.
@andrebattis941010 күн бұрын
I know that you heated the beaker before in the video. So I was wondering with that.
@Mohammad-obaidat-7210 күн бұрын
hello poor miner are purple stones telluride ore
@PoorMiners32110 күн бұрын
Brother, thats pyrite..
@Mohammad-obaidat-7210 күн бұрын
@@PoorMiners321 thank you bro but how can I recognize telluride stones and where to find them
@user-fl9ih9dy9y11 күн бұрын
Boss kailan pala dagdagan ng sulfuric acid pag natunaw na yung gold foil...puwedi ba yung tubig ng baterry ang idagdag
@PoorMiners32111 күн бұрын
Oo pag natunaw na, 10% lang man yung sulfuric na galing sa battery, kung walang sulfuric optional man lang yun pwedi naman wala bro..
@user-fl9ih9dy9y11 күн бұрын
@@PoorMiners321 ah boss segi subukan ko yan ang dami kung naipon ngayun na gold foil.mga nasa 50 grams.na
@PoorMiners32111 күн бұрын
@user-fl9ih9dy9y ang sulfuric kasi bro, pang precipitate man langvyun sa lead, pero kung gold foil ang tunawin mo wala ng lead yun kasi para saakin di na kailangan yun, ang dami, siguradohin mo yan,
@user-fl9ih9dy9y2 күн бұрын
Boss yung tinunaw ko na gold foil sa muriatic at hydrogen peroxide.pagkatapos nilagyan ko ng sodium metabulsulfite hindi bumaba ang sodium parang naging kulay brown yung tubig peru walang nalaglag sa ilalim na gold powder ano ang gagawin ko ditu boss dadagdagan kopa ulit ng sodium metabulsulfite patulong ako boss sayang yung pinagpaguran ko
@christopherleubner663311 күн бұрын
I just boil it down then filter. Make nitrated cofee filters as they are resistant to it and easily burn to recover the materials soaked in them. Then i keep cooking till it starts crystalizing let cool saving the gold as HAuCl4. This then gets fed into an electrolytic cell eventually that makes 3 or 4N gold plus chlorine that gets used to recover other noble metals. Also jewlers like the chloroauric acid to feed their electroplating machines and they pay more than the gold value for it. ❤
@PoorMiners32111 күн бұрын
Good to know brother, thanks
@andrebattis941012 күн бұрын
Hey bro I have a question and you are the man. I have AR that is pregnant with gold but also has base metals in it. Would adding sulfuric acid and heating it dissolve the base metals. So I can precipitate the gold?
@PoorMiners32112 күн бұрын
So add directly precipitant, i recommend iron sulfate to precipitate gold and leaving base metal in solutions.
@andrebattis941012 күн бұрын
Thank you
@andrebattis941011 күн бұрын
So should I heat the aqua regia because it's dark black. Then add iron sulfate. I have about 3 gallons of liquid.
@andrebattis941011 күн бұрын
Can I add smb instead
@andrebattis941011 күн бұрын
I watch your video when to stop added the smb. I added a little too much water to aqua regia that's why I wanted to know if I should heat til the brown fumes are gone. And some of the water will be reduced.
@shineyrocks39012 күн бұрын
Those look delicious
@Musallem77l12 күн бұрын
How is your health now? You said in a previous clip that you had an injury to your leg
@PoorMiners32112 күн бұрын
Thanks brother, He's okay brother, he's recovered after a month and a half from infection..
@Musallem77l12 күн бұрын
@@PoorMiners321 I wish you good health, brother
@PoorMiners32112 күн бұрын
Thanks brother, you too and God blees..
@yusonchavez708713 күн бұрын
Brother, Saan pwede omorder ng 31-36% HCL? at saka san pwede bumili ng Tin Chloride?
@PoorMiners32113 күн бұрын
31 to 36 mahirap hanapin yan bro, yung sa akin galing yun sa supplyer ng swemming pool, pero yung sa market na 29% maganda na yan bro yan yung gagamitin ko sa gold refining yung 29% lang, at yung tin chloride pwedi na ikaw na gumawa nyan bro 15 grams of pure tin metal, tutunawin mo sa 50ml 29%hcl yun na yun tin chloride.
@adeeladdi912613 күн бұрын
Hi, we are gold miner from Pakistan, can you give your WhatsApp contact details? We will discuss some interesting experiences
@gabrielheredia756314 күн бұрын
Great work 🎉
@junlee99314 күн бұрын
gold master
@PoorMiners32114 күн бұрын
Thanks
@rosauroruz292815 күн бұрын
Really poor,,,just a stove and a charcoal!inefficient daw sabi ng isa,,,e kaya nga ang caption poor miner,,
@user-nu2im8qq7i15 күн бұрын
dami ako yan bos pyrites
@PoorMiners32115 күн бұрын
Maganda yun sayo..
@preuischerherold740115 күн бұрын
Did you show thiosulfate leaching in a future video?
@PoorMiners32115 күн бұрын
Soon brother..
@volodymyrhrudetskyi65415 күн бұрын
Can you show differents between chalcopyrite and gold pls in video
@PoorMiners32115 күн бұрын
Yes brother we make it soon..
@filiposgioftsidis54916 күн бұрын
Can mercury capture microscopic gold particles that the ore may contains ? For example I have some ore containing tiny gold particles not bigger than 10μm , will mercury work with that ?
@PoorMiners32116 күн бұрын
Yes mercury can do it, but you need to apply presure..like moving the material..
@Anil_Gurung887416 күн бұрын
Hii
@keiverdejesusblancorodrigu926516 күн бұрын
Excelente amigo cuanta placa usaste
@PoorMiners32115 күн бұрын
obrigado amigo, não contei quantas peças eram, mas eram perto de três quilos
@gabrielheredia756317 күн бұрын
Tell me more of basalt and gold
@RobertWard-sb2ez17 күн бұрын
If I wouldn't have read the comments , I wouldn't have known what the hay he added!