I made mine with a rivet gun part and a wire .it worked.
@darrellphipps12206 ай бұрын
I make my own drippers out of aluminum bolts . I drill small holes with different small drill bits to get the desired size I want , very easy to do and you save a potload of money .
@joearledge16 ай бұрын
Pro tips: make sure you have a way to control the heat on the burner. Use pure lead for best results. Alloys, like range scrap, are more "runny" so pellets come out smaller than expected and less spherical. Pure lead also maximizes the weight per pellet. Wet tumble for 4 to 6 days(doesn't have to be all at once, 1day X 4 to 6, 2days X 2 to 3, ect...). Rinse with cold water to reduce oxidation, spread on towel to dry for a couple of days. Tumble with about 2.5CC of graphite powder per about 9lbs, for about 6 to 9 hours. Load and make ready.
@maddog45auto665 ай бұрын
A little tip, go to your local Napa car car park store and get mail threaded. Cand Take a drill press and drill the size of shot you want. It will save you a lot of money.
@harrisontaylor45316 ай бұрын
Hi, where is the follow up video from this ? I want to see your shot being made
@daveseip48095 ай бұрын
You won’t see it cause it don’t work I bought a machine and the lead doesn’t get round it’s more flat
@onetransmission78713 ай бұрын
When times get tough don't be bashful. You can use driveway gravel in a pinch. Just sayin'
@chrisvandonsel3656 ай бұрын
Semper fi mac!
@BuilderCannon9 ай бұрын
Hey saw your dacebook post so i said i give you a subscriber. What part of az are you from.
@ROBERTMADDEN1009 ай бұрын
I am in the west valley, Peoria
@kennethjohnson42844 ай бұрын
do u sell your shot,,if so do u have #4 shot?
@ROBERTMADDEN1004 ай бұрын
Sorry no I do not sell my shot.
@kennethjohnson42844 ай бұрын
ok just asking@@ROBERTMADDEN100
@onetransmission78713 ай бұрын
If you melt down lead use a wax toilet bowl ring to draw out impurities.
@ROBERTMADDEN1003 ай бұрын
You can also use a white candle or saw dust works really well also